Falling Dart Impact 2.60 - 7.20 J
1.92 - 5.31 ft-lb
Average value: 4.40 J Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..
Falling Dart Impact 5.20 - 7.20 J
3.84 - 5.31 ft-lb
Average value: 6.27 J Grade Count:3
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..