Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 542.328 - 542.328 J @Temperature -40.0 - -40.0 °C |
400.001 - 400.001 ft-lb @Temperature -40.0 - -40.0 °F |
Average value: 542 J Grade Count:1 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |