Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 2.80 J | 2.07 ft-lb | ASTM D3763 |
LNP Lubricomp® LL-4040 Polyetheretherketone, PTFE Additive
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |