Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | 13.4 J | 9.88 ft-lb | ASTM D3763 |
LNP Thermotuf® OF-1006 HI Polyphenylene Sulfide, Glass Fiber Reinforcement
(discontinued **) Features: High Impact ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades .. |