| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Dart Drop, Total Energy | 16.0 - 18.0 J | 11.8 - 13.3 ft-lb | Average value: 16.7 J Grade Count:3 |
| Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Multiaxial Impact Strength, Max Load, 2.2 m/s; ASTM D3763 |
| Mytex Polymers AS319L-01US Thermoplastic Polyolefin, 19% Talc Filled AS319L-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural or .. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
Multiaxial Impact Strength, Max Load, 2.2 m/s; ASTM D3763 |
| Mytex Polymers AS319LW-01US Thermoplastic Polyolefin, 19% Talc Filled AS319LW-01US is a compounded thermoplastic polyolefin (TPO) designed for exterior automotive applications requiring cold temperature impact, processability and paintability. Available in natural, g.. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics LNP LUBRICOMP DFL36EU PC LNP* Lubricomp* DFL36EU is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Easy Molding and UV Stabilized. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature -30.0 °C |
11.8 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics NORYL SE100X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/V1 rated. RTI Elec/Imp/Str 95/80/95. Good flow. Suitable for E/E market indoor/outdoor applications. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature -30.0 °C |
11.8 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics NORYL SE100X PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated FR resin. Improved productivity and reliability. 199F HDT. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Asia Pacific) 10% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics LNP STAT-KON OEL13I PPS - Linear LNP* STAT-KON* OEL13I is a compound based on PPS-Linear resin containing 15% Carbon Fiber, 5% PTFE. Added features of this grade include: High Impact, Wear Resistant, Electrically Conductive. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics LNP STAT-KON WEF42I PBT LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive. |
|||
| Dart Drop, Total Energy | 16.0 J | 11.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC LNP THERMOCOMP* DF004ER is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. Mold Release. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics LNP THERMOCOMP DF005 PC LNP* Thermocomp* DF005 is a compound based on Polycarbonate containing 25% Glass Fiber. |
|||
| Dart Drop, Total Energy | 16.0 J | 11.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics LNP THERMOCOMP JF004EXP PES LNP* THERMOCOMP* JF004EXP is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. |
|||
| Dart Drop, Total Energy | 16.0 J | 11.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics LNP THERMOCOMP TH0600A PUR LNP THERMOCOMP* TH0600A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
| Dart Drop, Total Energy | 16.0 J | 11.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics LNP THERMOCOMP TH0815A LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
| Dart Drop, Total Energy | 16.0 J | 11.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics LNP THERMOCOMP TH0815A PUR (Asia Pacific) LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics LNP THERMOCOMP WH0420A_GY5A749 PBT 4.2 specific gravity, PBT, gray |
|||
| Dart Drop, Total Energy | 16.0 J | 11.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East) LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics NORYL IGN320 PPE+PS 20% glass reinforced PPE + PS. High heat, high modulus automotive applications like ignition coils. |
|||
| Dart Drop, Total Energy | 16.0 J | 11.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics LNP STAT-KON DE003P PC LNP STAT-KON* DE003P is a compound based on Polycarbonate resin containing 15% Carbon Fiber. Added features of this material include: Electrically Conductive, Exceptional Processing. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics LNP THERMOCOMP RF008S PA 66 LNP* THERMOCOMP* RF008S is a compound based on Nylon 6/6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics LNP THERMOCOMP RX05494 PA 66 LNP* Thermocomp* RX05494 is a compound based on Nylon 6/6 resin containing glass fiber fillers. Added features of this material include: Heat Stabilized. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
| Dart Drop, Total Energy | 16.0 J @Temperature 23.0 °C |
11.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No.. |
|||
| Dart Drop, Total Energy | 16.0 J @Thickness 0.0500 mm |
11.8 ft-lb @Thickness 0.00197 in |
1100N; ISO 7765-2 |
| Borealis RD734CF Polypropylene Random Copolymer RD734CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD734CF is recommended for food packaging, high quality stati.. |
|||
| Dart Drop, Total Energy | 16.0 J | 11.8 ft-lb | Average value: 16.0 J Grade Count:3 |
| Overview of materials for Polycarbonate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
| Dart Drop, Total Energy | 16.0 J | 11.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics LNP THERMOTUF PF006I PA 6 LNP THERMOTUF* PF006I is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
| Dart Drop, Total Energy | 16.0 J | 11.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics LNP STAT-KON MFD02 PP LNP* STAT-KON* MFD02 is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
| Dart Drop, Total Energy | 16.0 J | 11.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
| SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific) LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||