Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP KONDUIT ITF2B PA 6/12 (Asia Pacific) LNP* Konduit* ITF2B is a compound based on Nylon 6/12 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Dart Drop, Total Energy | 8.00 J @Temperature -40.0 °C |
5.90 ft-lb @Temperature -40.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FL2000 PC Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa.. |
|||
Dart Drop, Total Energy | 8.00 - 20.0 J | 5.90 - 14.8 ft-lb | Average value: 14.9 J Grade Count:7 |
Overview of materials for Polyimide This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Dart Drop, Total Energy | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP FL003 PE LNP* LUBRICOMP* FL003 is a compound based on Polyethylene resin containing 15% PTFE. Added features include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL V01525 PPE+HIPS (Asia Pacific) Noryl* V01525 is a 15% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 LNP* LUBRICOMP* IFL34 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Dart Drop, Total Energy | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36L PA6.12 LNP* LUBRICOMP* IFL36L is a compound based on Nylon 6/12 containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Low Extractable, Wear Resistant. |
|||
Dart Drop, Total Energy | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 LNP* LUBRICOMP* RCL34 is a compound based on Nylon 66 containing 20% Carbon Fiber, 15% PTFE. Added features of this grade includes: Wear Resistant, Electrically Conductive. |
|||
Dart Drop, Total Energy | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36U PA 66 LNP* LUBRICOMP* RFL36U is a compound based on Nylon 66 resin containing 15% PTFE, 30% Glass Fiber. Added features of this grade include: Wear Resistant, UV Stabilized. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Asia Pacific) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DD000 PC (Europe-Africa-Middle East) LNP STAT-KON* DD000 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Dart Drop, Total Energy | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Dart Drop, Total Energy | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP AX04518 ABS LNP* THERMOCOMP* AX04518 is a compound based on ABS resin containing proprietary filler(s). |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC LNP THERMOCOMP* DF006ER is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DF0089 PC LNP THERMOCOMP* DF0089 is a compound based on Polycarbonate resin containing 40% Glass Fiber. Added features include: Flame Retardant. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP IC006 PA 6/12 (Asia Pacific) LNP* Thermocomp* IC006 is a compound based on Nylon 6/12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific) LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific) LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RF0029S PA 66 LNP* THERMOCOMP* RF0029S is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Dart Drop, Total Energy | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RX06421S PA 66 LNP* Thermocomp* RX06421S is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 Polyester, TP (Asia Pacific) LNP* Thermocomp* WC006 is a compound based on Polyester, TP resin containing Carbon Fiber. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
Dart Drop, Total Energy | 8.00 J @Temperature 23.0 °C |
5.90 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing 10% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant, Flame Retardant.. |
|||
Dart Drop, Total Energy | 8.00 J | 5.90 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON QEL329 PA 6/10 (Asia Pacific) LNP STAT-KON* QEL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 8.00 - 99.0 J @Temperature -30.0 - 0.000 °C |
5.90 - 73.0 ft-lb @Temperature -22.0 - 32.0 °F |
Average value: 76.7 J Grade Count:15 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |