Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C7210A PC+ABS (Asia Pacific) Cycoloy* C7210A resin is talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties. UL-94 V1 listed at 2.0mm intended for a wide range of different applications. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS Color package may affect performance. PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature -30.0 °C |
34.7 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS High impact and ductility at 73F and -20F. For thin-wall applications. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature -30.0 °C |
34.7 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics Cycoloy® C1110HF PC+ABS (Asia Pacific) PC+ABS, excellent flow/impact/high heat resistance. Suitable for thin wall application. Low temperature ductility (-20F). For automotive, appliance and electrical components. |
|||
Dart Drop, Total Energy | 47.0 J | 34.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC LNP* LUBRILOY* D20009P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant, Exceptional Processing... |
|||
Dart Drop, Total Energy | 47.0 J | 34.7 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC (Asia Pacific) LNP* Lubriloy* D20009P is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Flame Retardant,.. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP Cycoloy_C7210A PC+ABS LNP* Thermocomp* Cycoloy_C7210A isa a talc-filled PC+ABS, nonhalogenated FR for thinwall molding applications. Very good modulus-ductility balance. |
|||
Dart Drop, Total Energy | 47.0 J | 34.7 ft-lb | ASTM Test |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature 23.0 °C |
34.7 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Europe-Africa-Middle East) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Dart Drop, Total Energy | 47.0 J @Temperature -30.0 °C |
34.7 ft-lb @Temperature -22.0 °F |
Internal Testing |
CPC - Vycom PROTEC® Copolymer Polypropylene (CPP) Protec CP is one of various types of "impact copolymers"—a rapidly growing segment of the thermoplastic sheet market. In contrast to homopolymer polypropylene (which involves the polymerization of .. |