Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG38 ABS (Europe-Africa-Middle East) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG38F ABS Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG38F ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. FDA compliant. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG38N ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG38N ABS (Asia Pacific) Very high impact ABS. Toughness/rigidity. Good fatigue resistance. NSF Standard 61 certified in limited colors (restrictions may apply)> |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG47N ABS Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MG47N ABS (Asia Pacific) Multi-purpose, injection molding ABS providing a favorable balance of engineering properties. NSF Standard Multi-purpose, injection molding ABS providing a favorable balance of engineering properti.. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® MGABS01 ABS Injection molding ABS. High impact, high gloss, good flow. |
|||
Dart Drop, Total Energy | 31.0 J | 22.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing 10% Glass Beads and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 31.0 J | 22.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL SE100HX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated FR. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON MX12407C PP LNP* STAT-KON* MX12407C is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL N750 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL N850 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL N850 PPE+PS (Asia Pacific) ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical and Business Equipment applications. |
|||
Dart Drop, Total Energy | 31.0 J @Temperature 23.0 °C |
22.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX91077 PC LNP* STAT-KON* DX91077 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Impact Modified. |
|||
Dart Drop, Total Energy | 31.0 J | 22.9 ft-lb | ASTM D3763 |
Styrolution Terluran® EHI-4 NR ABS Extrusion Application Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Dart Drop, Total Energy | 31.0 J | 22.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX626 PPE+PS+PA Blowmolding and extrusion. High heat and chemical resistant. |
|||
Dart Drop, Total Energy | 31.0 J | 22.9 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC (Asia Pacific) LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |