Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY CR7020 ASA ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY CR7020 ASA (Asia Pacific) ASA copolymer. Profile/sheet coextrusion over ABS. Excellent weatherability, good flow/aesthetics and high impact. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 505RU PC Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East) Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE.. |
|||
Dart Drop, Total Energy | 25.0 - 70.0 J @Temperature -40.0 - -20.0 °C |
18.4 - 51.6 ft-lb @Temperature -40.0 - -4.00 °F |
Average value: 52.3 J Grade Count:49 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature -30.0 °C |
18.4 ft-lb @Temperature -22.0 °F |
Instrumented; ASTM D3763 |
LyondellBasell Hifaxâ„¢ CA244 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA244 high melt flow, 850 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has an excellent combination of stiffness, processability and dynamic.. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature -30.0 °C |
18.4 ft-lb @Temperature -22.0 °F |
Instrumented; ASTM D3763 |
LyondellBasell Hifaxâ„¢ CA387 Thermoplastic Polyolefin Elastomer Description: Hifax â„¢ CA387 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Paint.. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature -30.0 °C |
18.4 ft-lb @Temperature -22.0 °F |
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763 |
LyondellBasell Hifaxâ„¢ CB285 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB285 high melt flow, 1,300 MPa flexural modulus, low CLTE, UV-stabilized, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of .. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature 0.000 °C |
18.4 ft-lb @Temperature 32.0 °F |
Instrumented Energy at Maximum Load; ASTM D3763 |
LyondellBasell Hostacomâ„¢ TKS708D Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ TKS708D medium high melt flow, 1,300 MPa flexural modulus, UV-stabilized, high impact thermoplastic elastomeric olefin (TEO) resin has an excellent combination of propert.. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP YL003 Polyester Elastomer LNP* LUBRICOMP* YL003 is a compoudn based on Polyester Elastomer resin containing 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Dart Drop, Total Energy | 25.0 J | 18.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DEI13F PC (Asia Pacific) LNP* Stat-kon* DEI13F is a compound based on Polycarbonate resin containing Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Internally Lu.. |
|||
Dart Drop, Total Energy | 25.0 J | 18.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Dart Drop, Total Energy | 25.0 J | 18.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX05499 PC (Asia Pacific) LNP STAT-KON* DX05499 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® HX3061HP PBT PBT for compounding/fibers only. Not intended for injection molding. Biocompatible. Melt viscosity: 250C at 21.6 kgf is 1450-1850 poise. Available in Natural color (1001) only. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific) DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
Dart Drop, Total Energy | 25.0 J | 18.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6 LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing 40% Glass Fiber. |
|||
Dart Drop, Total Energy | 25.0 J | 18.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 25.0 J | 18.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 (Asia Pacific) LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 25.0 J | 18.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DEI13F PC LNP* STAT-KON* DEI13F is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 2% Silicone. Added features of this material include: Electrically Conductive, Superior Molding, Wear R.. |
|||
Dart Drop, Total Energy | 25.0 J | 18.4 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP PF008 PA 6 (Asia Pacific) LNP THERMOCOMP* PF008 is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOTUF PX07437 PA 6 Compound based on Nylon 6 resin containing glass fiber and impact modifier. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature -30.0 °C |
18.4 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL EM6101 PPE+PS Automotive interiors. Improved flow characteristics/overall processing economy. 250F DTUL. Good property retention/wide temperature range. |
|||
Dart Drop, Total Energy | 25.0 J @Thickness 0.0500 mm |
18.4 ft-lb @Thickness 0.00197 in |
1100 N force; ISO 7765-2 |
Borealis BA11CF Polypropylene Copolymer BA110CF is a heterophasic copolymer. This grade is suitable for use on chill roll processes. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. .. |
|||
Dart Drop, Total Energy | 25.0 J @Thickness 0.0500 mm |
18.4 ft-lb @Thickness 0.00197 in |
1200N; ISO 7765-2 |
Borealis Borseal™ RE239CF Polypropylene Copolymer Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high.. |
|||
Dart Drop, Total Energy | 24.9 J @Temperature -30.0 °C |
18.4 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
ExxonMobil Exxtral™ H1025W Performance Polyolefin Product Description: A polyolefin injection molding compound designed with good flow, cold temperature impact resistance, low CLTE, weatherable mold-in-color and also suitable for painted automotive.. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics GELOY CR7520 ASA (Asia Pacific) ASA copolymer. Automotive grilles and exteriors. Excellent weatherability, good flow/aesthetics and high impact. Rated f2 by UL. |
|||
Dart Drop, Total Energy | 25.0 J @Temperature 23.0 °C |
18.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36HL PC LNP LUBRICOMP* DFL36HL is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable, Healthcare. |