Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXE4472L PC (Asia Pacific) Lexan* FXE4472L is a 20% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL14 PC LNP LUBRICOMP* DFL14 is a compound based on Polycarbonate resin containing 20% Glass Fiber and 5% PTFE. Added features include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 23.0 J | 17.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 23.0 J | 17.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC (Asia Pacific) LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 23.0 J | 17.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC (Asia Pacific) LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 23.0 J | 17.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL23 PC LNP* Lubricomp* DFL23 is a compound based on Polycarbonate resin containing 15% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
Instrumented; ASTM D3763 |
LyondellBasell Hifaxâ„¢ CA287AHF Thermoplastic Polyolefin Elastomer Description: Hifax â„¢ CA287AHF is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Pa.. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763 |
LyondellBasell Hifaxâ„¢ ETA3081HS Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ ETA3081HS medium melt flow, 800 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has balanced physical properties, moldability and paintability. .. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature -30.0 °C |
17.0 ft-lb @Temperature -22.0 °F |
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763 |
LyondellBasell Hifaxâ„¢ HSBMR246 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ HSBMR246 medium high melt flow, 1,500 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an outstanding balance of physical pro.. |
|||
Dart Drop, Total Energy | 23.0 J | 17.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DP0039EF PC (Asia Pacific) LNP* Lubricomp* DP0039EF is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DC10EPFR PC LNP* STAT-KON* Lexan_DC10EPFR is a compound based on Polycarbonate containing Carbon Fiber. Added features of this grade include: Exceptional Processing, Flame Retardant, Electrically Conductive. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON TE002 PU LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Valox® IQ3001 PBT Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Dart Drop, Total Energy | 23.0 J | 17.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
Dart Drop, Total Energy | 23.0 J | 17.0 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOTUF DF008EI PC (Asia Pacific) LNP* Thermotuf* DF008EI is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release, High Impact. |
|||
Dart Drop, Total Energy | 23.0 J @Thickness 0.0500 mm |
17.0 ft-lb @Thickness 0.00197 in |
1100; ISO 7765-2 |
Borealis BD712CF Polypropylene Copolymer BD712CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD712CF is recommended for food packaging.. |
|||
Dart Drop, Total Energy | 23.0 J @Thickness 0.0500 mm |
17.0 ft-lb @Thickness 0.00197 in |
1180 N; ISO 7765-2 |
Borealis BorPURE™ RD208CF Polypropylene Random Copolymer BorPure™ RD208CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. This grade is suitable for the manufacturing of unoriented films o.. |
|||
Dart Drop, Total Energy | 23.0 J @Temperature 23.0 °C |
17.0 ft-lb @Temperature 73.4 °F |
Gardner Falling Dart Impact (GFDI); ASTM D5420 |
LyondellBasell Hostacom™ ZG750 Polypropylene Copolymer Description: Hostacom™ ZG750 conventional melt flow, 1,700 MPa flexural modulus, 40% calcium carbonate-filled, utility grade polypropylene copolymer resin has a very good combination of strength, s.. |