Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 94.0 J @Thickness 3.20 mm |
69.3 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1201-05 Polycarbonate Resin Description: LUPOY PC 1201-05 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Dart Drop, Total Energy | 94.0 J @Thickness 3.20 mm |
69.3 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1261-03 Polycarbonate Resin Description: LUPOY PC 1261-03 resin is designed for extrusion blow molding(EBM) and injection stretch blow molding (ISBM) products. It exhibits an excellent physical property balance of heat resista.. |
|||
Dart Drop, Total Energy | 94.0 J @Thickness 3.20 mm |
69.3 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1302-05 Polycarbonate Resin Description: LUPOY 1302-5 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main.. |
|||
Dart Drop, Total Energy | 94.0 J @Thickness 3.20 mm |
69.3 ft-lb @Thickness 0.126 in |
203m/min; ASTM D3763 |
LG Chemical Lupoy 1300-03 Polycarbonate Resin Description: LUPOY PC 1300-03 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |