Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL4000U PC (Asia Pacific) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL4000U PC (Europe-Africa-Middle East) Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific) Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul.. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® R9453 PC (Asia Pacific) Lexan* R9453 Polycarbonate (PC) is a non-filled, non-chlorine and non-brominate flame retardant resin for general purpose, which contains 30% post-consumer recycled PC. This resin is of UL-94 V0 rat.. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East) XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East) XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Asia Pacific) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT3141 PC Copolymer (Europe-Africa-Middle East) XHT3141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Asia Pacific) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Europe-Africa-Middle East) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® BFL4000U PC Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo.. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Asia Pacific) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
Dart Drop, Total Energy | 68.0 J @Temperature 23.0 °C |
50.2 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Europe-Africa-Middle East) Low-medium flow, suitable for blow molding, injection molding, extrusion. |
|||
Dart Drop, Total Energy | 68.0 J | 50.2 ft-lb | ASTM D3763 |
Lubrizol ISOPLAST™ 302EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |