Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® EX39F ABS Highest impact extrusion ABS for sheet and blow molding applications. FDA food contact compliant. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific) Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Asia Pacific) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® EXL4016H PC Copolymer (Europe-Africa-Middle East) 6% GF reinforced opaque polycarbonate-siloxane copolymer with good impact strength, stiffness and hydrolytic stability. |
|||
Dart Drop, Total Energy | 39.0 J | 28.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC LNP* LUBRICOMP* DL001 is a compound based on Polycarbonate resin containing 5% PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 39.0 J | 28.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DL001 PC (Asia Pacific) LNP* Lubricomp* DL001 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON TX06488NTX1 PU LNP* STAT-KON* TX06488NTX1 is a compound based on Polyurethane resin containing Proprietary Filler(s). Added features of this grade are: Execllent Ductility, Electrically Conductive. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature -30.0 °C |
28.8 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature -30.0 °C |
28.8 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX910 PPE+PS+PA (Asia Pacific) Unfilled grade for automotive on-line painted components. Dimensional stability. Excellent chemical resistance. Class A surface appearance. |
|||
Dart Drop, Total Energy | 39.0 J | 28.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL N225X PPE+PS PPE+PS blend. Unfilled. Halogen-Free FR performance. UL94 V0/5VA. UL746C F1. Dielectric Strength. Suitable for E/E market indoor/outdoor applications. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Asia Pacific) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DX02437 PC (Asia Pacific) LNP Stat-Kon DX02437 is a compound based on Polycarbonate resin containing conductive carbon powder, with good impact-resistance, flow and ESD performance, suitable for semi-con industry. |
|||
Dart Drop, Total Energy | 39.0 J | 28.8 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL EZ250 PPE+PS Automotive wheel covers. Offers superior processability/flow and better chemical resistance when exposed to many automotive fluids over PX0844. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycolac® EX39 ABS Highest impact extrusion ABS for sheet and blow molding applications. |
|||
Dart Drop, Total Energy | 39.0 J @Temperature 23.0 °C |
28.8 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL ENG265 PPE+PS PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a.. |