Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 3.00 - 7.00 J @Temperature -30.0 - -20.0 °C |
2.21 - 5.16 ft-lb @Temperature -22.0 - -4.00 °F |
Average value: 3.75 J Grade Count:3 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati.. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics NORYL SE100HX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated FR. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 LNP* LUBRICOMP* IL004 is a compound based on Nylon 6/12 resin containing 20% PTFE. Added features of this material include: Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal LNP LUBRICOMP* KP004 is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK LNP* LUBRICOMP* LL004C is a compound based on Polyetheretherketone resin containing 20% PTFE. Added features of this material include: Wear Resistant, Clean Compounding System. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP LL004C PEEK (Asia Pacific) LNP* Lubricomp* LL004C is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated, Clean Compounding System. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Branched (Asia Pacific) LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched LNP* LUBRICOMP* OFL36A is a compound based on PPS - Branched resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763 |
SABIC Innovative Plastics SABIC PPCOMPOUND 37T1020 PP SABIC® PPcompound 37T1020 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits high impact and high flow, and is suitable for injection mold.. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RL002 PA 66 LNP LUBRICOMP* RL002 is a compound based on Nylon 66 resin containing 10% PTFE. Added features of this material include: Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RL004S PA 66 LNP LUBRICOMP* RL004S is a compound based on Nylon 66 resin containing 20% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RP004S PA 66 LNP* LUBRICOMP* RP004S is a compound based on Nylon 66 containing PTFE/Silicone. Added features of this grade include: Heat Stabilized, Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP RX99518 PA 66 LNP* LUBRICOMP* RX99518 is a compound based on PA66 containing Proprietary Fillers. Added feature of this material is: Wear Resistant. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT LNP* LUBRICOMP* WL0049 is a compound based on PBT containing 20% PTFE. Added features include: Wear Resistant, Flame Retardant. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP ZX05506 PPE+PS (Asia Pacific) LNP LUBRICOMP* ZX05506 is a compound based on PPE+PS Blend resin containing Graphite Powder, PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON KX02764 Acetal LNP STAT-KON* KX02764 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-LOY AX06484 ABS LNP* STAT-LOY* AX06484 is a compound based on ABS resin containing Talc. Added feature of this grade is: Antistatic, Extrudeable. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature -30.0 °C |
2.21 ft-lb @Temperature -22.0 °F |
Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP 9X07430 PBT+PC LNP* THERMOCOMP* 9X07430 is a compoud based on a PBT+PC Blend containing Glass Fiber, Talc. Added features of this material include: Opaque, Weatherable. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP LNP THERMOCOMP* MB006S is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific) NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific) LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON OE006A PPS - Branched LNP STAT-KON* OE006A is a compound based on PPS - Branched resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-LOY W3000XXJ PBT LNP* STAT-LOY* W3000XXJ is a compound based on PBT. Added features of this grade include: Anti-Stat, Colorable, Healthcare |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC LNP* THERMOCOMP* DB0049F is a compound based on Polycarbonate resin containing 20% Glass Bead. Added features of this material include: Flame Retardant, Superior Molding. |
|||
Dart Drop, Total Energy | 3.00 J | 2.21 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP DB0049F PC (Asia Pacific) LNP* Thermocomp* DB0049F is a compound based on Polycarbonate resin containing Glass Bead, Flame Retardant. Added features of this material include: Flame Retardant, Superior Molding. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GTX EXNX0080 PPE+PPS (Europe-Africa-Middle East) Noryl APS* EXNX0080 resin is a glass filled, high performance blend of PPE/PPS that exhibits an excellent balance of high-heat resistance, strength, flame retardant, and conductivity. This grade can.. |
|||
Dart Drop, Total Energy | 3.00 J @Temperature 23.0 °C |
2.21 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics Lexan® 3412HF PC (Asia Pacific) 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |