Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP FARADEX NS003 PC+ABS LNP* FARADEX* NS003 is a compound based on PC+ABS resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL349EF PC LNP LUBRICOMP* DFL349EF is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated. |
|||
Dart Drop, Total Energy | 15.0 - 56.0 J | 11.1 - 41.3 ft-lb | Average value: 39.5 J Grade Count:4 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DZL34E PC (Asia Pacific) LNP* Lubricomp* DZL34E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Dart Drop, Total Energy | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DE003 PC (Asia Pacific) LNP STAT-KON* DE003 is a compound based on Polycarbonate resin containing Carbon Fiber. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DE004 PC (Asia Pacific) LNP STAT-KON* DE004 is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific) LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON MX01739C PP LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP AF002 ABS LNP THERMOCOMP* AF002 is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP JF004 PES LNP THERMOCOMP* JF004 is a compound based on Polyethersulfone resin containing 20% Glass Fiber. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66 LNP* THERMOCOMP* RC006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Dart Drop, Total Energy | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Dart Drop, Total Energy | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Dart Drop, Total Energy | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Asia Pacific) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DD0009PC PC LNP STAT-KON* DD0009PC is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP STAT-KON DE003ER PC (Asia Pacific) LNP STAT-KON* DE003ER is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP AF002XXC ABS LNP THERMOCOMP* AF002XXC is a compound based on ABS resin containing 10% Glass Fiber. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA 66 (Asia Pacific) LNP* Thermocomp* RC006 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP UF009S PPA LNP THERMOCOMP* UF009S is a compound based on Polyphthalamide resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Dart Drop, Total Energy | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP THERMOCOMP YF005 POLYESTER ELASTOMER LNP* THERMOCOMP* YF005 is a compound based on Polyester Elastomer resin containing 25% Glass Fiber. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP VERTON RV00AES PA 66 (Europe-Africa-Middle East) LNP VERTON* RV00AES is a compound based on PA 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Dart Drop, Total Energy | 15.0 J @Temperature 23.0 °C |
11.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA LNP* VERTON* UX03320 is a compound based on Polyphthalamide resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | 1200N; ISO 7765-2 |
Borealis Bormed™ SC820CF Polypropylene Random Copolymer Bormed™ SC820CF is a very soft random heterophasic copolymer. Applications: Bormed™ SC820CF is recommended for packaging for medical devices. Bormed™ SC820CF contains no slip, antiblock, antist.. |
|||
Dart Drop, Total Energy | 15.0 J | 11.1 ft-lb | Instrumented Impact Energy @ peak; ASTM D3763 |
SABIC Innovative Plastics LNP LUBRICOMP DBL349E PC (Asia Pacific) LNP* Lubricomp* DBL349E is a compound based on Polycarbonate resin containing Glass Bead, PTFE, Flame Retardant. Added features of this material include:LNP* Lubricomp* DBL349E is a compound based .. |