Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 293 MPa @# of Cycles 1.00e+7 |
42500 psi @# of Cycles 1.00e+7 |
rotating beam |
Carpenter Gall-Tough PLUS™ Stainless, Annealed Data provided by Carpenter Technology Corporation.6.4 mm diameter tensile specimens from center of 25.4 mm diameter bar annealed 1066°C 1 hour, water quenched, and ground.Threshold Galling Stress 4.. |
|||
Fatigue Strength | 293 MPa @# of Cycles 1.00e+7 |
42500 psi @# of Cycles 1.00e+7 |
rotating beam |
Carpenter Gall-Tough PLUS™ Stainless, Annealed, 0% Cold Work Data provided by Carpenter Technology Corporation.Annealed 1150°C, water quenched, and cold drawn.Threshold Galling Stress 48 MPa. The avg. total volume loss on the wear test is 10.6 mm³ at 100 r.. |