Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 85.0 MPa @# of Cycles 1.00e+6 |
12300 psi @# of Cycles 1.00e+6 |
10 Hz, ASTM Type I tensile bar |
Solvay Specialty Polymers Ryton® R-4 02XT Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-4 02XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve ducti.. |
|||
Fatigue Strength | 85.0 MPa @# of Cycles 1.00e+7 |
12300 psi @# of Cycles 1.00e+7 |
R.R. Moore Test, Smooth Rotating Beam |
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |