Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 460 MPa | 66700 psi | Limit; test specifics not reported |
TIMET 8-1-1 Titanium Alloy (Ti-8Al-1Mo-1V); Annealed Sheet Industry Specifications: USA Aerospace: AMS 4915,4916. France: T-A8DV. Features: Designed for creep resistance up to 450°C, used primarily in engine applications such as forged compressor blades.. |