Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 350 MPa @# of Cycles 1.00e+8 |
50800 psi @# of Cycles 1.00e+8 |
rotating beam (Aging - 595°C/16 h F.C. to 540°C, AC) |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC.. |