Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Fatigue Strength | 241 MPa | 35000 psi | Strip (TH04) |
CMW® 100 Copper Alloy CMW® 100 material is a heat treatable, high strength, high conductivity copper base alloy. Its properties are a combination of highest strength and hardness with relatively high electrical and ther.. |
|||
Fatigue Strength | 241 MPa | 35000 psi | Rod & Bar |
CMW® 73 Copper Alloy CMW® 73 material is a heat treatable copper base alloy having extremely high hardness and strength coupled with fair electrical and thermal conductivity. The extremely high hardness, strength and w.. |
|||
Fatigue Strength | 241 MPa | 35000 psi | endurance limit; test details not reported |
ATI Allegheny Ludlum Stainless Steel Type 301, annealed (UNS S30100) Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho.. |