Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 150 MPa @Load 36.5 kg |
21800 psi @Load 80.5 lb |
cond.; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg |
21800 psi @Load 80.5 lb |
dry; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 MCS V0 Polyamide 6 - Flame Retarded, Unreinforced Flame retarded (class V0), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th.. |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg |
21800 psi @Load 80.5 lb |
dry; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 MCS V2 Polyamide 6 - Flame Retarded, Unreinforced Flame retarded (class V2), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th.. |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg |
21800 psi @Load 80.5 lb |
cond.; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 GF40 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 40% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg |
21800 psi @Load 80.5 lb |
dry; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 MCS 850 Polyamide 6 - Flame Retarded, Unreinforced Glow wire resistance 850°C, bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has .. |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg |
21800 psi @Load 80.5 lb |
dry; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 MCS Polyamide 6 - Colored Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.For colored parts produced by injection molding.Tarnamid® has the following .. |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg |
21800 psi @Load 80.5 lb |
dry; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 MHLS Polyamide 6 - Colored Heat and UV light stabilized grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main proper.. |
|||
Ball Indentation Hardness | 150 MPa @Load 36.5 kg |
21800 psi @Load 80.5 lb |
dry; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-30 MHLS Polyamide 6 - Colored High viscosity heat and UV light stabilized grade for injection molding.Tarnamid® has the following main properties:High mechanical strength, rigidity and hardnessHigh impact strengthHigh vibration.. |