Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 70.0 MPa @Load 36.5 kg |
10200 psi @Load 80.5 lb |
cond.; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 MCS V2 Polyamide 6 - Flame Retarded, Unreinforced Flame retarded (class V2), bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has th.. |
|||
Ball Indentation Hardness | 70.0 MPa @Load 36.5 kg |
10200 psi @Load 80.5 lb |
cond.; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 MCS 850 Polyamide 6 - Flame Retarded, Unreinforced Glow wire resistance 850°C, bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has .. |