Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 19.3 kN/m @Temperature 99.0 °C |
110 pli @Temperature 210 °F |
resistance to glass; ASTM D3167 |
Huntsman KRYSTALFLEX® PE 505 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |