Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.175 kN/m @Temperature 230 °C |
1.00 pli @Temperature 446 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9085 Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.175 kN/m @Temperature 230 °C |
1.00 pli @Temperature 446 °F |
Adhesion on Aluminum; ASTM D3330 |
3M 9085UV Ultra High Temperature 100 HT Adhesive Transfer Tape 3M™ Ultra High Temperature 100HT Adhesive Transfer Tapes 9082 and 9085 utilize a high performance and low outgassing adhesive system having excellent heat resistance in high temperature environment.. |
|||
Peel Strength | 0.175 kN/m @Temperature 82.0 °C |
1.00 pli @Temperature 180 °F |
180° |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |