Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 4.56 kN/m @Temperature 121 °C |
26.0 pli @Temperature 250 °F |
T-Peel, 90 min @ 350°F, Spring Clamp Pressure, FPL Acid Etched 6061-T6; ASTM D1876 |
Zyvex Performance Materials Aroply™ 350 Nano-Engineered Composite Film Adhesive Aroply™ 350 Film Adhesive is a versatile, heat curing carbon-nanotube modified epoxy structural film adhesive available in a variety of film weights on a supported carrier. Cured adhesive character.. |
|||
Peel Strength | 4.56 kN/m @Temperature 82.2 °C |
26.0 pli @Temperature 180 °F |
Bell Peel |
Hexcel® Redux® 609 (0.06 psf) Adhesive film for bonding metallic and composite components Redux 609 is a 250°F curing modified epoxy film adhesive containing a cottom scrim for easy handling and glue-line thickness control. It is available at standard areal weights of 0.06 psf and 0.04 .. |
|||
Peel Strength | 4.56 kN/m @Temperature 60.0 °C, Time 605000 sec |
26.0 pli @Temperature 140 °F, Time 168 hour |
JRF/SW, Stainless Steel; AMS-S83318 |
3M AC-250 A-1/6 Aerospace Sealant 3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l.. |
|||
Peel Strength | 4.56 kN/m @Temperature 60.0 °C, Time 605000 sec |
26.0 pli @Temperature 140 °F, Time 168 hour |
JRF, Alodine; AMS-S83318 |
3M AC-250 A-1/6 Aerospace Sealant 3M Aerospace Sealant AC-250 A-1/6 is a two-part, low temperature curing polysulfide, quick repair sealant for integral fuel tank and fuselage sealing applications. The mixed compound is a pourable l.. |
|||
Peel Strength | 4.56 kN/m @Temperature 24.0 °C, Time 259000 sec |
26.0 pli @Temperature 75.2 °F, Time 72.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1099-L Nitrile High Performance Plastic Adhesives Features: It is a low viscosity grade for spray application.Fast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions and sheeting. (Ma.. |
|||
Peel Strength | 4.56 kN/m @Temperature 82.0 °C, Time 1.81e+6 sec |
26.0 pli @Temperature 180 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1300 Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |
|||
Peel Strength | 4.56 kN/m @Temperature 24.0 °C, Time 605000 sec |
26.0 pli @Temperature 75.2 °F, Time 168 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |
|||
Peel Strength | 4.56 kN/m @Temperature 24.0 °C, Time 605000 sec |
26.0 pli @Temperature 75.2 °F, Time 168 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |
|||
Peel Strength | 4.56 kN/m @Temperature 24.0 °C, Time 259000 sec |
26.0 pli @Temperature 75.2 °F, Time 72.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 4491 Nitrile Industrial Adhesive Features: Low viscosity grade for spray applicationFast dryingProvides strong, flexible bondsResists weathering, water, fuels, oil and plasticizersBonds vinyl extrusions and sheeting (May stain ligh.. |
|||
Peel Strength | 4.56 kN/m @Temperature 24.0 °C, Time 259000 sec |
26.0 pli @Temperature 75.2 °F, Time 72.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives Features: It is a medium viscosity grade for most brush or flow applicationsFast dryingProvides strong, flexible bonds.Resists weathering, water, fuels, oil and plasticizers.Bonds vinyl extrusions a.. |
|||
Peel Strength | 4.56 kN/m @Temperature 82.0 °C, Time 1.81e+6 sec |
26.0 pli @Temperature 180 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1300L Neoprene High Performance Rubber Gasket Adhesives 3M™ Scotch-Weld™ Neoprene High Performance Rubber ^& Gasket Adhesives 1300 is the most versatile of our rubber and gasket adhesives. They may be used to bond metal, wood, most plastics, and neopre.. |