Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.28 kN/m @Temperature 24.0 °C, Time 259000 sec |
13.0 pli @Temperature 75.2 °F, Time 72.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 10 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 10 is a multi-purpose contact adhesive which may be used to bond plastic laminate, aluminum, steel, wallboard, wood, masonry, rubber and canvas.Informati.. |
|||
Peel Strength | 2.28 kN/m @Temperature -34.0 °C, Time 1.81e+6 sec |
13.0 pli @Temperature -29.2 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1357 Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |
|||
Peel Strength | 2.28 kN/m @Temperature -34.0 °C, Time 1.81e+6 sec |
13.0 pli @Temperature -29.2 °F, Time 504 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 1357-L Neoprene High Performance Contact Adhesive 3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrat.. |
|||
Peel Strength | 2.28 kN/m @Temperature 14.0 °C, Time 86400 sec |
13.0 pli @Temperature 57.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847 Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 2.28 kN/m @Temperature 14.0 °C, Time 86400 sec |
13.0 pli @Temperature 57.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847-H Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsHigh viscosity grade adhesive for many brush or spray applications.Quick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |
|||
Peel Strength | 2.28 kN/m @Temperature 24.0 °C, Time 86400 sec |
13.0 pli @Temperature 75.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 4475 Industrial Adhesive Features: Dries quickly to a firm bondExcellent resistance to water, plasticizer migration, many detergent and soap solutions, oils and greasesA general purpose adhesive for bonding most vinyls, cer.. |
|||
Peel Strength | 2.28 kN/m @Time 605000 sec |
13.0 pli @Time 168 hour |
T-Peel, Canvas/Canvas, aged 2 days @ 49°C, Freon #11 |
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive Features: A light colored, fast drying adhesiveExcellent resistance to aromatic fuels, water and oilUsed to bond many types of plastic films including ABS, cellulose acetate, and PVCInformation prov.. |
|||
Peel Strength | 2.28 kN/m @Temperature 14.0 °C, Time 86400 sec |
13.0 pli @Temperature 57.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 847-L Nitrile High Performance Rubber & Gasket Adhesive Features: Strong flexible bondsMedium viscosity grade adhesive for many brush or flow applicationsQuick dryingExcellent resistance to many fuels and oilsBond leather, nitrile rubber, most plastics, .. |