Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 13.4 kN/m @Temperature 24.0 °C |
76.5 pli @Temperature 75.2 °F |
Metal-to-metal |
Hexcel® HexPly® F185 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F185; Fiber: 75-1/0Information provided by HexCel |
|||
Peel Strength | 13.4 kN/m @Temperature 82.0 °C |
76.5 pli @Temperature 180 °F |
Metal-to-metal |
Hexcel® HexPly® F185 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F185; Fiber: 75-1/0Information provided by HexCel |