Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 560 MPa @Thickness 25.0 - 76.2 mm |
>= 81200 psi @Thickness 0.984 - 3.00 in |
Tempers T651 / T652 |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Tensile Strength | 560 MPa @Thickness 50.0 - 60.0 mm |
81200 psi @Thickness 1.97 - 2.36 in |
Typical Strength |
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |