Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 55.2 MPa @Temperature 150 °C |
8010 psi @Temperature 302 °F |
ASTM D638 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Tensile Strength | 55.2 MPa @Temperature 150 °C |
8010 psi @Temperature 302 °F |
ASTM D638 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Tensile Strength | 55.2 MPa @Temperature 90.0 °C |
8010 psi @Temperature 194 °F |
ASTM D638 |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |