Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 55.2 MPa @Temperature 23.0 °C |
8000 psi @Temperature 73.4 °F |
ASTM D638 |
Saint-Gobain Meldin® 7022 CM Compression Molded Graphite Filled Polyimide Melidin® 7022 CM is a compression molded polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin.. |
|||
Tensile Strength | 55.2 MPa @Temperature 23.0 °C |
8000 psi @Temperature 73.4 °F |
ASTM D638 |
Saint-Gobain Meldin® 7211 DF Direct Formed Graphite and PTFE Filled Polyimide Melidin® 7211 DF is a direct formed polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Specific.. |