Polymer Property : Tensile Strength = 3770 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 26.0 - 30.0 MPa

@Temperature 50.0 °C
3770 - 4350 psi

@Temperature 122 °F
DuPont™ Tedlar® SP TXX10AH9 Polyvinyl Fluoride Film
Colored, High Gloss. Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the superb durability, color stability, chemical resistance,..
Tensile Strength 26.0 MPa

@Strain 20.0 %,
Temperature 100 °C
3770 psi

@Strain 20.0 %,
Temperature 212 °F
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..