Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 225 MPa @Diameter 20.0 - 40.0 mm |
32600 psi @Diameter 0.787 - 1.57 in |
|
United Cast Bar Unibar 250 Continuously Cast Iron Offers a good combination of strength and wear resistance, while still possessing good machinability and produces excellent surface finishes. Noise and vibration damping are excellent in this grade... |
|||
Tensile Strength | 225 MPa @Diameter 150 - 300 mm |
32600 psi @Diameter 5.91 - 11.8 in |
|
United Cast Bar Unibar 350 Continuously Cast Iron Unibar 350 is a special grade alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and producing a.. |