Polymer Property : Tensile Strength = 18100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 125 MPa

@Strain 5.00 %,
Temperature 80.0 °C
18100 psi

@Strain 5.00 %,
Temperature 176 °F
5mm/min
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
Tensile Strength 125 MPa

@Temperature 70.0 °C,
Time 1.44e+6 sec
18100 psi

@Temperature 158 °F,
Time 400 hour
62% RH
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled
In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele..