Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 586 - 724 MPa @Thickness <=25.4 mm |
85000 - 105000 psi @Thickness <=1.00 in |
Cold Drawn Bars |
Schmolz + Bickenbach UGIMA® 304 Cu Stainless Steel Bar Description: 304Cu UGIMA® is an enhanced machining grade produced only by Ugitech, providing the ultimate level of machinability available in an non-resulfurized austenitic stainless steel. 304Cu.. |