Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 86.2 MPa @Temperature 23.0 °C |
12500 psi @Temperature 73.4 °F |
ASTM D638 |
Saint-Gobain Meldin® 7001 CM Compression Molded Polyimide Meldin® 7001 CM unfilled polyimide base resin, compression moldedSpecification Qualifications:Satisfies Type I P for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide .. |