Polymer Property : Tensile Strength = 590 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 590 MPa

@Thickness 25.0 - 76.2 mm
85600 psi

@Thickness 0.984 - 3.00 in
Typical Strength
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..
Tensile Strength 590 MPa

@Thickness 6.50 - 12.0 mm
85600 psi

@Thickness 0.256 - 0.472 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Tensile Strength 590 MPa

@Thickness 12.0 - 25.0 mm
85600 psi

@Thickness 0.472 - 0.984 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..