Polymer Property : Tensile Strength = 560 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 560 MPa

@Thickness 25.0 - 76.2 mm
>= 81200 psi

@Thickness 0.984 - 3.00 in
Tempers T651 / T652
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..
Tensile Strength 560 MPa

@Thickness 50.0 - 60.0 mm
81200 psi

@Thickness 1.97 - 2.36 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..