Tensile Strength 550 MPa

@Diameter 105 - 200 mm
79800 psi

@Diameter 4.13 - 7.87 in
United Cast Bar Unibar 600-3 Continuously Cast Spheroidal Graphite Iron
Offers reasonable machinability and excellent surface finish combined with higher wear resistance, strength & heat treatment. Noise and vibration damping are good in this grade.Unibar 600-3 can be ..
Tensile Strength 550 MPa

@Diameter 205 - 600 mm
79800 psi

@Diameter 8.07 - 23.6 in
United Cast Bar Unibar 600-3 Continuously Cast Spheroidal Graphite Iron
Offers reasonable machinability and excellent surface finish combined with higher wear resistance, strength & heat treatment. Noise and vibration damping are good in this grade.Unibar 600-3 can be ..
Tensile Strength >= 550 MPa

@Thickness 76.2 - 127 mm
>= 79800 psi

@Thickness 3.00 - 5.00 in
Tempers T651 / T652
Constellium Alumold® 500 Rolled Aluminum
The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop..
Tensile Strength 550 MPa

@Thickness 25.0 - 100 mm
79800 psi

@Thickness 0.984 - 3.94 in
Typical Strength
Constellium Certal® Thick Aluminum Plate
Certal® thick plates have been optimized to provide excellent machinability, shape stability and high strength. Certal® is therefore ideal for industrial tools. Applications include injection and ..
Tensile Strength >= 550 MPa

@Thickness 25.0 - 40.0 mm
>= 79800 psi

@Thickness 0.984 - 1.57 in
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..