Polymer Property : Tensile Strength = 370 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 370 MPa

@Diameter 105 - 200 mm
53700 psi

@Diameter 4.13 - 7.87 in
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Strength 370 MPa

@Diameter 205 - 600 mm
53700 psi

@Diameter 8.07 - 23.6 in
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Strength 370 MPa

@Diameter 105 - 200 mm
53700 psi

@Diameter 4.13 - 7.87 in
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Strength 370 MPa

@Diameter 205 - 600 mm
53700 psi

@Diameter 8.07 - 23.6 in
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Strength >= 370 MPa

@Thickness 60.0 - 80.0 mm
>= 53700 psi

@Thickness 2.36 - 3.15 in
Temper T451; Standard EN 485-2
Constellium ALPLAN® 2017A High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
ALPLAN® 2017A precision plates combine a very good dimensional stability with a high level of mechanical strength and elongation. The outstanding flatness, the low roughness and high quality of the..