Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 30.0 MPa @Temperature 121 °C |
4350 psi @Temperature 250 °F |
50%RH; ASTM D638 |
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612
(Unverified Data**) Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers |
|||
Tensile Strength | 30.0 MPa @Strain 1.00 %, Temperature 23.0 °C |
4350 psi @Strain 1.00 %, Temperature 73.4 °F |
ISO 527 |
BASF Ultramid® B3S HP PA6 (Dry) Ultramid B3S HP is a easy flowing, finely crystalline, injection molding PA6 for fast processing |
|||
Tensile Strength | 30.0 MPa @Strain 1.00 %, Temperature 150 °C |
4350 psi @Strain 1.00 %, Temperature 302 °F |
ISO 527 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |