Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 123 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 123 MPa

@Temperature 300 °C
>= 17800 psi

@Temperature 572 °F
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6
High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH
Copyright © lookpolymers.com All Rights Reserved