Mechanical Properties Metric English Comments
Tensile Strength 1140 MPa

@Diameter 0.838 mm
165000 psi

@Diameter 0.0330 in
unannealed, drawn from annealed 0.080" wire
H.C. Starck NRC® 91 Tantalum - 7% Tungsten Alloy
Applications: NRC® 91 Metal wire products are primarily used for their superior tensile and yield strengths and torsion modulus. These properties are retained at high temperatures in vacuum. F..