Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 68.0 kJ/m² @Temperature 23.0 °C |
32.4 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Sax Polymers SAXAMID 126F4RZ21 Nylon 6, 20% Glass Fiber SAXAMID 126F4RZ21 is a polyamide 6 injection-molding-grade reinforced with 20% glass fibers. It is equipped with a halogen-free and phosphorus-free flame retardant.Information provided by SAX Polyme.. |
|||
Izod Impact, Unnotched (ISO) | 68.0 kJ/m² @Temperature -30.0 °C |
32.4 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
Sax Polymers SAXAMID 226F6 Nylon 6.6, 30% Glass Fiber SAXAMID 226F6 is a general purpose polyamide 6.6 injection-molding-grade reinforced with 30% glass fibers. It has very high mechanical strength in combination with good flow properties. It shows hig.. |