Modulus of Rupture 0.421 GPa
61.0 ksi
Meehanite GE-30 Flake Graphite Cast Iron
Type GE-30 combines improved strength and solidity with higher machining feeds and speeds than ordinary gray iron.General Meehanite information - Meehanite metal is first melted to a definite degree..