Polymer Property : Modulus of Rupture = 2.03 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0140 GPa

@Treatment Temp. 725 °C
2.03 ksi

@Treatment Temp. 1340 °F
Pyrotek Pyrocast XL Small Component Refractory
ApplicationsThimbles Transition plates Down Spouts Control Pins Auto pour Ladles Strip Casting Nozzles AdvantagesThermal shock resistance High erosion resistance High service temperature Smooth cast..