Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.0120 GPa @Treatment Temp. 540 °C |
1.74 ksi @Treatment Temp. 1000 °F |
|
Pyrotek Pyrocast AR-S Castable Refractory Pyrocast AR-S is a low cement, fused silica, castable refractory which exhibits excellent resistance to thermal shock. It is inert to liquid aluminum and its alloys. It is a high strength material.. |