Polymer Property : Modulus of Rupture = 0.510 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00352 GPa
0.510 ksi
Dry Modulus of Rupture, 50% clay/50% flint, cast bars
Old Hickory Thomas Tennessee Ball Clay
Thomas clay is similar to Volunteer clay and has established an excellent history of performance in stoneware and low fire (talc base) plastic and casting formulas. The diverse combination of clays ..