Mechanical Properties Metric English Comments
Modulus of Rupture 0.00310 GPa
0.450 ksi
Dry Modulus of Rupture, 50% clay/50% flint, cast bars
Old Hickory Dunn Tennessee Ball Clay
Dunn clay is a selection originating from our Gleason, TN processing facility and is characterized by moderately high levels of kaolin interspersed with the presence of some carbon content. It is an..
Modulus of Rupture 0.00310 GPa
0.450 ksi
Extruded 50/50 Clay/Flint
Imerys Diamondâ„¢ Kaolin
Diamond is an intermediate-grained montmorillonitc kaolin used primarily in plastic formed bodies. This kaolin is known for its good strength and white-firing characteristics.Information provided by..
Modulus of Rupture 0.00310 GPa
0.450 ksi
Green (typ.)
Unifrax Fiberfrax® Duraboard® 500ES Ceramic Fiber Board
Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard ..
Modulus of Rupture 0.00310 GPa
0.450 ksi
Parallel
Zircar Ceramics NKO Castertip
Main stay "low mass hard tip" used on all makes of continuous thin strip aluminum casting equipment. NKO is a rigid combination of refractory ceramic fiber and inorganic binders. Information provid..