Polymer Property : Modulus of Rupture = 0.160 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00110 GPa
0.160 ksi
parallel to thickness
Zircar Refractory Composites ZIRCAL-18 Refractory Board
Type ZIRCAL-18 Refractory Board is a high temperature calcium silicate block insulation with excellent mechanical properties and stability up to 1100°C(2000°F). Its high thermal insulating value m..