Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.00100 GPa | 0.145 ksi | EN 993-6: 1995 |
Skamol Group V-LITE 475 Vermiculite Insulating Brick V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica.. |
|||
Modulus of Rupture | 0.00100 GPa | 0.145 ksi | EN 993-6: 1995 |
Skamol Group Moler SM-65 Insulating Block SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str.. |
|||
Modulus of Rupture | 0.00100 GPa @Temperature 815 °C |
0.145 ksi @Temperature 1500 °F |
ASTM C268 |
BNZ Materials Blazecrete 2800 Dense Castable Blazecrete 2800 is an economical, high alumina refractory for service to 2800°F (1556°C). Suitable for door linings, curbs and covers, pre-cast shapes, grey iron ladles, aluminum reverberatory fur.. |
|||
Modulus of Rupture | 0.00100 GPa | 0.145 ksi | ASTM C133 |
BNZ Materials BNZ-23HS Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Modulus of Rupture | 0.00100 GPa | 0.145 ksi | ASTM C133 |
BNZ Materials BNZ-25 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |